beneficiation process for concentrating abu tartur rock
Beneficiation of egyptian abu tartur phosphate rock. bioleaching of abu tartur phosphate ore by using . a.niger for 50 ml medium, 0.5 abu tartur phosphate ore incubated at 30 176c. different carbon and nitrogen sources were evaluated which peptone was the best